[MW:34749] PTC requirement as per ASME Sec VIII Div. 2

Hi All,

We are constructing two storage spheres as per ASME Sec VIII Div.2 with A516 Gr. 70 & A553 Type 1 material respectively. 

For A516 Gr. 70 material sphere (21m Dia, Weld length - 670m) with a single WPS-SMAW having PWHT for pressure part joints of Category A & B. Will Six no. PTC in vertical position qualify ASME Sec VIII Div. 2 requirements?

For A553 Type 1 material sphere (23.8m Dia, Weld length - 120m(1G), 222m(2G), 300m(3G), 300m(4G)) having 4 nos. WPS-SMAW (Client Spec requirement) for pressure part joints of Category A & B. 
1G - 1 No.
2G - 2 Nos.
3G - 3 Nos.
4G - 3 Nos.
PTC quantity as per above will qualify ASME Sec VIII Div. 2 requirements?

Kindly share your valuable views.

Thanks in advance.

Kind Regards,
Anish R
+971563518645

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/49c044c9-0247-4592-a5f2-9c77be416167n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...