Friday, January 5, 2024

[MW:34730] Hot and in catalyst reformer tube

Hi,
Hot band have been observed in reformer tube due to catalyst void.

Please share the information about which type of damage mechanism suspect in tube in this case.


Regards
Manish Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k7%3DbMZBzyzas6rN4AFyL3FCRYu_Pf97EptSn6tUKs1M4g%40mail.gmail.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...