With reference to subject having 2 queries regarding API 5L seamless pipes :

1. What is the exact differentiation between Pipe Grade & Steel Grade referred for PSL 2 Pipes? Unable to figure out exact difference.
2. What is the heat treatment cycle to be followed for the various heat treatments referred to in API 5L i.e. for Normalizing, Q&T, TMCP etc ?

--
With Regards,
Pravin Mohite.
Cell - 9664232573.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADC2jB2pf7K597g29hJ0PnmE17bYYh4JKBtJaLz5WHeb7nr1nQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...