Re: [MW:34646] Filler

both are except usage of shielding gas. C- For 100%CO2. M- Mixed gas. example Argon plus Co2 etc

On Fri, Nov 24, 2023, 9:16 PM Elayaraja Thangarasu <elayaraja1312@gmail.com> wrote:
Dear All.

 What is the difference E71T-1C and E71T-1M.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMsS8imTvKcoyfMPr43Wc7uex78s%3De0gOJ_JF8fKHnY_XKa19Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN6qvecbhhm5BSszLydnz2Pm9RDApK-NvTr6Rcz7yRr4g%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...