Wednesday, November 1, 2023

[MW:34621] Regarding welding consumable for Material CuNi 90/10 (P34) to hastelloy C276(P43)

Dear All,
I have one query regarding welding compatibility of material combination -  CuNi 90/10  UNS C70600 (P34) TO  Hastelloy C276 material UNS NO: N10276 (P43)It is weldable ?
If it is weldable, then please suggest welding consumable.


Regards,

Rahul U.


--