Re: [MW:34641] Interpretation QW202.2 b

yes, Maximum to be welded because test coupen thickness is 40mm

On Fri, Nov 24, 2023, 5:28 PM SANJAY SINGH <sanjay.kharwar349@gmail.com> wrote:
Dear One and All ,
               Please let me know QW 202 .2 b  actual interpretation  for partial penetration .

I have WPS  with Base metal thickness of 40 mm then whether it qualifies for partial weld groove above 200 mm Thk. base metal thickness also .





Regards 
Sanjay 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALkBf%2Bvnq_Vf5cGmGMoLe99grjVwvGZt%2BvRUxip50bgitDHtDQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePgNPn4Q%2BzUhZf%3DAxhBA41ZqX1NJ4xDDC7QPFMBgWV-MQ%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...