asme sec 1
On Fri, Nov 24, 2023, 5:28 PM Ashish Chacko <iamashleo007@gmail.com> wrote:
Dear Sirs,
I have inquiries regarding the comprehension of interpass temperature in ASME :
- 1)What code reference is used to ascertain the maximum interpass temperature?
- 2)What code reference is employed to establish the interpass temperature for dissimilar welds, such as CS to SS welds?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c2f3530-e9f7-4d0f-a51f-40f799445bdbn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM1RBjTWAY8w4r6QwEgq1o4ANmNx5J-pg_p8etifAnM8w%40mail.gmail.com.
Comments