Plate qualified welder can not weld pipe below 24", yes he can weld above 24" on pipes
On Sat, 4 Nov 2023 at 14:37, sachin sunny N <sachinsunnyn25@gmail.com> wrote:
Dear Experts,Does a welder qualified on plate can do weld on pipe as per ASME? What is the range for that?--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb81cef5-8919-4571-8ada-9222906f059dn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkFLjYjYYXJLePZvAbN2CpkU2Mtt7ybroezLOUJBKKqbfq%3D6w%40mail.gmail.com.
Comments