Re: [MW:32781] Iridium-192 Radiography

60mm with IR192... There after we have to carry out the RT by Cobalt 60.....


Regards..
Rishikesh Shahi
HOD QA/QC 
M/S FABTECH ENGINEERING PVT. LTD. NAGPUR, MAHARASHTRA 

On Mon, 24 Jan 2022, 3:06 pm Manish Kumar, <mkmkr431@gmail.com> wrote:
Dear Sir,
As per which, ASME clause or BARC regulatory, How much thickness of radiography can be carried out from Iridium 192 source. 

--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5eBcnvrHW-eO86oNUsxgc19YoViaTT3U9TfMSjMzu1HQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFf3VQNNRMPYzgaee-Fv_jC_1QUP7W9i7Bm9uN-xp6DD9J%2BXXw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...