Re: [MW:32765] skipping of PWHT (SR) and Hydrotest

Dear friend,

If joint welding of SS+ CS with 32mm thickness - as per ASME sec VIII div 1 for p no :1 PWHT is mandatory.
> if you preheated the CS side as per code? if the HAZ hardness on CS plate is within the base metal range, you can avoid PWHT process if end customer is accepting  this condition 
  

Regards,
Sankaran.SP
Welding & Metallurgy expert
coimbatore, India.  


On Wednesday, 19 January, 2022, 11:41:11 am IST, Shahil Saini <sainishahil98@gmail.com> wrote:


Hello everyone,

If the weld performed is sound on the 32 mm thik material (SS and CS) and preheated as per code, then can i skip the PWHT and Hydrotest??

Regards,
Shahil Saini
PGET-Welding 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-_JBJx8S4Yph3nt%3DoC0e%2BvKMd1RMA_6hfowNBTaGKyEA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...