If our Nominal Thickness Exceed by 38 mm, Then we have to perform PWHT,
For Nominal Thickness Definition See UW-40
Thanks & Regards
Avanish Kumar Singh
On Wed, Jan 19, 2022, 1:35 PM Shahil Saini <sainishahil98@gmail.com> wrote:
Hello everyone,--If 4-5 mm welding is performed in the 32 mm thick material, is PWHT & Hydro required or not or can I skip PWHT and Hydro? any clause related to this??Regards,Shahil SainiPGET-Welding
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9cFtaCVyaygJ4L8gXRqSVXs_L8PYTzOMYKOidgcOYVeQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKwEcjgxW0%2B5rKN6S9erkXnR1-mUwZxsmUgFrmc%2BRhGY6NHseg%40mail.gmail.com.
Comments