If the weld performed is sound on the 32 mm thik material (SS and CS) and preheated as per code, then can i skip the PWHT and Hydrotest??

Regards,
Shahil Saini
PGET-Welding 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-_JBJx8S4Yph3nt%3DoC0e%2BvKMd1RMA_6hfowNBTaGKyEA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...