Thursday, July 22, 2021

Re: [MW:32455] Consumable Required to weld base Metal A516 Gr-70

70 KSI is the  minimum UTS  of SA 516 GR 70.

So all consumables shall have 70 KSI minimum  UTS.

For said mentioned consumables in below your mail ,  70 KSI minimum  is achieved for consumables.
So no problem at all.
Get WPS PQR reviewed approved before start of production Welding.

On Thu, 22 Jul 2021, 15:58 Muhammad Azeem, <azeem7999@gmail.com> wrote:
Gents,
I need your kind assistance to explain the consumable can be used for this material, As I received from one vendor WPS with following consumable from root till fill/cap. As I know the tensile strength of the base metal is 70000 KSI So  consumable should have more ??

Root - ER-70S-2 -GTAW
Fill - E7018 - SMAW
EH12K/F7P8- SAW

Regards,

M.Azeem Iqbal
 0590071467

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2fad85f4-5b42-44cb-9eb8-357c9414dfc3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MEU%2Baf6zgcafOedR2F_J6JO%2BBYA0%3DAjqaQy9RC--OPwg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...