Monday, July 19, 2021

Re: [MW:32453] When is supplementary essential variable becomes Essential ?

When Notch Toughness requirements are specified, then supplementary essential variables become  Essential variable. 
Regards

On Mon, 19 Jul 2021, 08:20 PK M, <pkmqaqc@gmail.com> wrote:
Dears,

When does the supplementary essential variable become Essential ? 

thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfYY8%3D0_GwfXjVnFFbjQU%3Dc-z1ugVsNjKzVpsvF-yS5JQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Nwc6odf%3DZo3MFptR5d%3DK-qGVSLo0LKrQeeVsqMAK6X%2Bg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...