Re: [MW:32452] When is supplementary essential variable becomes Essential ?

Supplementary Essential variable is to be considered and addressed in PQR/WPS when the WPS is qualified with CHARPY IMPACT test and whenever the material requires IMPACT TEST per code/standard.
Thanks,
MANIVANNAN.P

On Mon, Jul 19, 2021 at 8:20 AM PK M <pkmqaqc@gmail.com> wrote:
Dears,

When does the supplementary essential variable become Essential ? 

thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfYY8%3D0_GwfXjVnFFbjQU%3Dc-z1ugVsNjKzVpsvF-yS5JQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMrenNDDnPJHyzi9kbN3K_G%3D51Uy5JqG_auOcafynMZiRWcheA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...