Monday, July 12, 2021

Re: [MW:32448] Defects in welding

THope.this question is from India.
This is called Warm hole porosity.
This is typical surface defect of FCAW process and gets aggravated in moist environment.
Now a days there is rainy season in India .so atmosphere has a lot of moisture .
Pl specify Which brand is being used?

As I recall TASETO make wire are better when FCAW E309LT1 is used. 




On Mon, 12 Jul 2021, 07:45 Aditya Gujar, <gujar.adi@gmail.com> wrote:
Dear Experts,

We are facing defects in the stainless steel welding as per attached images, kindly let me know what could be the reason. 

Please note below information,

Consumable type: SMAW
Grade:E309LT1-1
Base metal: E309L plate
Co2 gas flow: 15-18
V: 28V
Current: 180-200 amps

Same batch of flux cored wire E309LT1-1 has worked just fine on the other jobs with similar applications. 

Thanks in advance. 

Regards, 
--
--
 
Aditya Gujar

---

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB89cpD8ioE8j-dUpwY4F7%3DLm0nDmB51tPLmongiwMG%2B0DvPzw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NAz9KKXZOnUa_3MK1p-dpxdNq7zCHE4iVNP1SfHyRcGA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...