Try cleaning with an SS wire brush .. Followed by cleaning with solvent like acetone .Better to use chloride ( halide ) controlled acetone 

On Mon, 17 May 2021 at 09:15, rajesh...@gmail.com <rajeshreddy32@gmail.com> wrote:
Hi All,

We are also facing the same issue in SDSS welds on 6" Pipe welded with ER2594.

Can anybody let me know the root cause for this spots and remedy. 

On Wednesday, February 12, 2014 at 3:08:50 PM UTC+5:30 Vasantharao wrote:
Dear Experts,

We observe Dark spots on Welding of Duplex Stainless Welds.  

Material is : UNS S31803 ,  Filler Wire for root - ER2594, rest ER2209.

Sample pictures are attached for reference.

Oxygen level in shielding / Purging maintained well below 0.2%.

Interpass <150 Deg.C

Pl. share your valuable information.

Thank you.

P.Rao

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6bd891d9-b534-41c5-99b1-3e07fde9894cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Og_YBsV8GhtFfnEmcfJEvtVYY%3DFshfTTZW3T7V8ccX7bg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...