Re: [MW:32389] PREHEAT TEMPERATURE

Min and Max preheat temperatures are mentioned in ASME Sec II C also for certain consumables.

Regards

Prem Nautiyal 


On Sun, 23 May 2021, 09:14 Manoj Mumbai, <manojacgnr@gmail.com> wrote:
ASME B31.3 and RP582

On Sat, May 22, 2021 at 3:26 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Could you give code ref for control of preheat on maximum side

On Sat, May 22, 2021, 3:10 PM Gerry Lourens <Gerry.Lourens@newage-eng.com> wrote:

There are no limits to the Preheat temperature provided that there are no toughness requirements.
If toughness (impacts) are required :
the maximum inter-pass temperature qualified equals the maximum preheat temperature.

Best Regards,

 

Gerry Lourens

Welding Engineer

New Age Engineering Solutions

 

M: +27 62 192 1207

T:  +27 17 631 5282

F:  +27 (0)86 616 9701

E:  gerry.lourens@newage-eng.com

A:  3 York Street, Evander, 2280

On Sat, May 22, 2021 at 5:49 AM Manoj Mumbai <manojacgnr@gmail.com> wrote:
Dear Experts,

The preheat temperature shall not be less than 55 deg. C as per QW-406.1 but  not specified a maximum how much it can be from the temperature noted in PQR as preheat temperature is minimum temperature and interpass temperature is the maximum temperature.
My question , Is there any limitation to increase preheat temperature than mentioned in PQR. suppose PQR temperature is Ambient, say 38 deg. C, can we increase preheat temperature to 204 deg. C.  I have a qualified procedure of P6 material at ambient temperature 38 deg.C now I have to include preheat temperature.

Thanks in advance for your expert opinion.
Manoj.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5%3DH94mRN3EHOgHBCxM3%2BuEJp3uqYP6qOrOjVbzrD0_bxg%40mail.gmail.com.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFgehWe%3DgfP78ODmmJBmWd%2B28HhfBD3Jtk5tC2SrYbt%2B7x0SGA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNv8zRKZ%2Bi-yZcPoKKGAGVOE4WfO_cztr3s8k4T5sXJtw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5mUfYrriofY2QSXT26TX%2BQ86CE513z8Uq1CSFcXQc3QqA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEP2HKCwvFNtTZJi7GN15XCroJLYvBFp31vtXfxcjXpZMRq%3DPA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...