Re: [MW:32354] WPS re qualification require If electrode brand/manufacturers change as per API 1104

According to API 1104 only Welding consumables with G classification like ER70SG, E7018G, E8010G etc..       as below highlighted require new PQR for change in manufacturer or Trade name.


Inline image

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 4 May, 2021, 08:49:04 am IST, HARISH VARUDE <harish.varude02@gmail.com> wrote:


Dear experts,

With reference to above subject please update me...

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YK%2B9Jocd1N7Cmq1DkE7uGgYFMzXD7pvj4RnikR_hoQFxqg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...