Re: [MW:32353] WPS re qualification require If electrode brand/manufacturers change as per API 1104

Hi sir,
I don't think so,
Please see the below:

"5.4.2.6 Filler Metal
The following changes in filler metal constitute essential variables:
a) a change from one filler metal group to another (see Table 1);
b) for materials with a SMYS greater than or equal to that of the material specified as API 5L Grade X65, a change in
the AWS classification of the filler metal (see 5.4.2.2).
Changes in filler metal within filler metal groups may be made within the material groups specified in 5.4.2.2. The
compatibility of the base material and the filler metal should be considered from the standpoint of mechanical
properties."


Vào Th 3, 4 thg 5, 2021 vào lúc 10:12 HARISH VARUDE <harish.varude02@gmail.com> đã viết:
Dear experts,

With reference to above subject please update me...

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YK%2B9Jocd1N7Cmq1DkE7uGgYFMzXD7pvj4RnikR_hoQFxqg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OmBGtMweF%3DzpKS8S9Cmk%2Bv6kG8iPsks0apM1fNhu7D%2Bow%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...