[MW:32355] filler material between 304L and 316L

Dear Experts,

     At the site 308L filler wire used for the Pipe joint between 304L and 316L.  After doing the PMI QC rejected the joints and suggesting to use 316 filler.

   Experts kindly share the details of the code reference to accept or any procedure to avoid cutting 20joints.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0xA0VB5ScFArEbYRJMODF7D%2B0dwsfdrL4qO1GygpVXhzg%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...