Monday, December 23, 2019

Re: [MW:30310] Why 2’’ Dia and below size can’t be partially repaired

Dear Sir, 

Note: Comments based on ASME B31.3 Code

No such restrictions in code as per my knowledge.

We does partial repairs, but the only thing is one should be confident enough to mark the repair based on a DWDI (Ellipse) RT film. 

Regards, 

Hareesh K V

On Mon, Dec 23, 2019, 4:34 PM Venkadesh Lakshmanan <venkadeshmech@gmail.com> wrote:
Gents,

Could you please provide any spec reference regarding 2'' and below size pipe Welding can't be partially repaired.

Regards,
Venkadesh 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_6cSfWXXDgtPxGFo-P9h7dmgu_UXUyaA%3DCyjTejx%3Dna1kz9w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEv1fk-WQ4MtaD_hoSyhXLdegGYNwoYGpd2oMRShj%3DPa4S86Cw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...