[MW:30295] Preheat temperature of EN10025 S 275 JR and S355JR

Dear Experts,

I have to weld S275 JR and S355JR  of unlimited thickness as per AWS D1.1 but the material are unlisted material.  In Table 4.9 the unlisted material preheat temperature is not shown but in WPS what temperature I should provide and on what basis.

Thanks in advance

Manoj,
Welding Inspector.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nJDi7gOCwBAP407QNfe011tzX4PsxJdpwD69b9jgPqsg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...