Please select one joint for RT out of 10 joints welded
We are following this practice here in saudi Aramco
We are following this practice here in saudi Aramco
Mohammed Tajuddin
On Sat, 7 Dec 2019, 8:40 am Aakash, <harenathjha@gmail.com> wrote:
Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01379daa-22dd-4bfd-ae0b-335e77f9e8d5%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACZrEUb%3D_trgLnxoQDyYR-%3D%2BpPt6DCi-TE5da%3DZuwrKSMYY%2BsA%40mail.gmail.com.
Comments