[MW:30307] Why 2’’ Dia and below size can’t be partially repaired

Gents,

Could you please provide any spec reference regarding 2'' and below size pipe Welding can't be partially repaired.

Regards,
Venkadesh 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_6cSfWXXDgtPxGFo-P9h7dmgu_UXUyaA%3DCyjTejx%3Dna1kz9w%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...