ER 70s

On Thu, Dec 19, 2019 at 3:01 PM NILESH <nileshkaranje1010@gmail.com> wrote:
Dear experts,
We have pipe line having material API 5L X70 PSL2, dia.8"X 12.7mm, which filler wire for GTAW welding ?
Thanks in advance for your comments. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a239a49-36b2-452b-931e-d4d57800dd74%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJBR2%2BOzRMQYf8urrOVm4ganzjeEW%2BjtCi4ae-cxSV1SqTKnfA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...