-- when we carryout PQR for material A 312 TP 321 welding to A312 TP 321 (pipe 8'' SCH 120)
1. Welding Process GTAW+SMAW
2.Welding consumable ER347+E347-16
3.Interpass max 175 oC
4.pwht :900 Celsius at 8 hours
5. Code applied ASME
problems: 2 side Bend test were broken
Can some body know or have experience above problem
Tuan
QA/QC posco
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments