Re: [MW:21700] Which is Suitable consumable (Filler wire and Flux) for SA 516 Gr 70 plate

Dear Mr. Gobalakrishnan
 
There is no Impact requirement
 
Thanks & Regards,
 
Mohamed Ali Samsudeen


On Saturday, 23 August 2014 7:53 PM, Gopalakrishnan G <gopal2408@gmail.com> wrote:


is there any Impact requirement? specify thickness details


On Fri, Aug 22, 2014 at 11:23 AM, 'Mohamed ali' via Materials & Welding <materials-welding@googlegroups.com> wrote:
pls  ignore previous mail


Dear Expert 
Which is Suitable consumable (Filler wire and Flux) for SA 516 Gr 70 plate for Tank welding by Automatic Girth welding, SAW process.  No PWHT.
i have suggest EM12K - F7A8, Is it correct or wrong.  


 
Thanks & Regards,
 
Mohamed 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...