Hi
They are stress relief checks and are common in hardfacing.
Regards
Prem Nautiyal
cell: 9769316004
On Saturday, August 30, 2014 10:07 AM, jsn <jsn@cal2.vsnl.net.in> wrote:
Dear ,
Can please explain why hair line cracks are appearing after welding with ahand facing electrode
I have used a build up electrode layer - 2
and 1 or two layers with hard facing electrode a hair line crack at varius intervals.
I am informed that since it is hardfacing electrode hair line cracks will appear
= s p raman=
J.Suryanarayanan
J.Suryanarayanan
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments