please check Test certificate of your electrode (impact value specified by manufacturer) and what is the interpass temp maintained? more heatinput may also affect your impact.


On Sat, Aug 23, 2014 at 11:19 AM, 'CHINTUKUMAR GANDHI' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts,

Greetings of the day.

I came to an issue in WPQR of P No. 1 Group 2 Base metal in CVN Impact testing of weld and haz. Design Code is ASME Sec. VIII Div. 1 Ed. 2013 & ASME Sec. IX Ed. 2013.

Base Metal Thk. 25 mm. SA 516 Gr. 70
PWHT: Normalizing at 920+/-10º C.
Holding Period 65 Minutes.
Welding Process SMAW (Manual)
Electrode Used: 3.15 & 4.0 mm. E7018-1 (Impact tested in as welded condition).
Position: 3 G Uphill (Stringer/ Weave Bead)

CVN Impact test results of HAZ: 
Test Temp. -57º C (Temp. reduction applicable)
Specimen size: 10 x 5 x 55 mm.
Values in Joules HAZ Top Side- 5, 19.5, 4 (Average 9.50)
Values in Joules HAZ Bottom Side- 4.5, 4, 17.5 (Average 8.67)
Values reqd. for sub size specimen: Individual min. 8 J & Min. Average 10 J.

CVN Impact test results of Weld:
Test Temp. -46º C (Temp. reduction applicable)
Specimen size: 10 x 10 x 55 mm.
Values in Joules - 9, 14.5, 8.5 (Average 10.67)
Values reqd. for Std. size specimen: Individual min. 16 J & Min. Average 20 J.

What shall be the reason of failure? Is electrode selection OK?

Awaiting for your prompt favorable response at the earliest.

Thanks & regards,


C. R. GANDHI

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
G.Gopalakrishnan
Welding Engineer
Mukand Ltd
Mumbai
Moble :+91-9833397917

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...