Tuesday, August 26, 2014

Re: [MW:21702] Table 4.5 34) ---AWS D1.1

Hi,
It simply means that when you CANNOT take away backgouging/backing from a wps, but you are free to include backgouging/backing in your wps. When a procedure is qualified with backgouging/backing, your wps will always be with backgouging/backing either ceramic, or permanent. But when you have a PQR without backgouging/backing you are free to include this procedure in your wps.
Hope it clarifies.
From: sutthipong .k <leonard_pick@hotmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, 26 August 2014, 9:08
Subject: [MW:21700] Table 4.5 34) ---AWS D1.1

Dear All
 
                  Please explain in table 4.5 34) The omission, but not inclusion, of backing or backgouging.
 
If i have PQR qualification test CJP single V butt joint with ceramic backing.
Question.
                     1.) Can i write WPS range qualify to backing gouging CJP double V or Single V butt joint.?
                     2.) And, if i have PQR qualified with back gouging, Can i write WPS range qualify with ceramic backing or not.?
 
 
Best regard.
Sutthipong.K
QA/QC Welding.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...