Dear Mr.Ali
 
Yes we can.
Please refer below
 

QW-404.33 A change in the filler metal classification

within an SFA specification, or, if not conforming to a

filler metal classification within an SFA specification, a

change in the manufacturer's trade name for the filler metal.
 

QW-254

WELDING VARIABLES PROCEDURE SPECIFICATIONS (WPS)

Submerged-Arc Welding (SAW)

QW-404.33 - Classification  - is coming under Nonessential variables

 

 
Regards
K.Govindan
 
 

Date: Fri, 26 Apr 2013 11:21:41 +0400
From: mhaskar.aly@gmail.com
To: materials-welding@googlegroups.com
Subject: [MW:17560] Use of other brands of filler & Flux combination for SAW welding than what brand used during PQR

Dear Friends
 
We have PQR with F7A8 EM12K from ESAB Brand ;
 
Can we use F7A8 EM12K from other Brands viz Bohler, Lincoln, Kiswel etc...
 
Is it acceptable as per SEC IX...
 
 
Ali Mhaskar
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...