Re: [MW:17547] SAW PIPE ( PSL2) FOR SKELP HYSDROTEST AT THE TIME OF MPQT/REGARING MECHNICAL TEST SAMPLE

Dear Alam,

Yes,it's required the pipe shall withstand the hydrostatic test without leaked through the weld seam or pipe body ( API SPECIFICATION 5L )

RGDS,

Zulfan

SeAH Steel Corp



On Wed, Apr 24, 2013 at 2:17 AM, sajidalam mohd. <engineer_makes_world@yahoo.co.in> wrote:
DEAR ALL
                GOOD DAY
I WANT TO KNOW FOR CARBON STEEL PIPE-PSL-2 (SAW WELDING) SKELP PORTION/SKELP PIPE SHOULD BE HYDRO TESTED OR NOT AT THE TIME OF MPQT.

THE SAMPLE FOR MECHANICAL TEST  SHOULD BE HYDRO TESTED  OR NOT IN SAW WELDED PIPE???ITS MANDATORY THAT SAMPLE FOR MECHANICAL TEST SHOULD BE HYDRO  TESTED IN SAW PIPE /PSL-2 DURING PRODUCTION AND AT THE TIME OF MPQT?PLEASE GIVE REFERENCES OF CODE AND STD.

REGARDS
MD S ALAM
MECH ENGINEER
DAMMAM-SAUDI

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...