Re: [MW:17506] Welder validity

verify his continuity and allow to work by y contractor



On Mon, Apr 22, 2013 at 12:56 PM, joseph mbé <mbejoseph@yahoo.fr> wrote:
contractor working for manufacturer!!!!!!!! Any way, Contractor or manufacturer shall be responsible for conducting the performance test as per QW300.2;  the welder can only work under the supervision of the responsible (contractor or manufacturer) thus, Y contractor shall requalified the welder in accordanc with the applicable standard.
 
Jo F Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
 

De : HAREESH K V <hareesh13h@gmail.com>
À : materials-welding <materials-welding@googlegroups.com>
Envoyé le : Lundi 22 avril 2013 6h20
Objet : Re: [MW:17502] Welder validity
Now as the manufacturer is same there is no need of re qualification, because the welder is welded under the quality guidelines of the manufacturer not the contractor X or Y.

Please refer QW 300.2 (a) of ASME BPVC Sec IX.

Now if the manufacturer itself is working under the quality guidelines of different clients, then the welder has to be re-qualified.

Hope for comments if i am wrong, with references.
On Sun, Apr 21, 2013 at 4:49 PM, Nirmal kumar Mondal <nkmp.mondal@gmail.com> wrote:
he need again to qualified as a new employer.
On Sun, Apr 21, 2013 at 3:39 PM, Prakash Hegde <pb.hegde@yahoo.com> wrote:
He need requalification as his employer is cahnged so his Identification is changed
Regards
 
Hegde --- On Sat, 20/4/13, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:

From: Maulik Thakkar <mlkthakkar2@gmail.com>
Subject: [MW:17489] Welder validity
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 20 April, 2013, 9:25 PM

Dear all,
Query- one qualified welder under x contractor at one manufacturer. Now consider he left the x contractor & join y contractor & working under same manufacturer but at different location.
In view of above case is he qualified to do welding under y contractor at same manufacturer located at different place?......or need requalification?
Regards, MHT
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm   The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com. For more options, visit https://groups.google.com/groups/opt_out.    
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm   The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com. For more options, visit https://groups.google.com/groups/opt_out.    
--
----------------------
Hareesh K V
+91-9447625012

-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm   The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com. For more options, visit https://groups.google.com/groups/opt_out.    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...