Creep strength is the ability of a metal to withstand a constant force at elevated temperatures. At elevated temperature, material with small grain size will be prone to phenomenon of grain boundary sliding (as smaller the grain size, the larger will be the total boundary surface area per unit volume). Therefore material with larger grain will give better creep properties.

According to my (little) knowledge:

Small grain size→ high hardness, tensile strength, yield strength

Intermediate grain size → high toughness, good fatigue properties

Large grain size→ high creep strength, ductility


Regards,

Ali Samdani



On Wed, Apr 24, 2013 at 8:08 PM, Dr-alaa Zg <dralaazg@yahoo.com> wrote:
Greetings...

Creep is different failure mode, creep strength will be better as the grain size increased. The reason behind such behavior is that as the grain becomes coarse, grain boundary area will be minimized.

Dr. Eng. Alaa Abdulhasan Atiyah
UOT- Baghdad- iraq


From: selastine sudhakar <mechselastine@gmail.com>;
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>;
Subject: [MW:17550] creep strength vs grain size
Sent: Wed, Apr 24, 2013 4:09:19 PM

Dear experts

What is the relation between grain size and creep strength..

Thanks
selastine

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...