Saturday, July 19, 2025

Re: [MW:35724] Abridged summary of materials-welding@googlegroups.com - 2 updates in 1 topic

Redo the Hydrotest after the PWHT and NDT.

Regards,

On Fri, Jul 18, 2025 at 2:11 AM <materials-welding@googlegroups.com> wrote:
Kannayeram Gnanapandithan <kgpandithan@gmail.com>: Jul 17 02:05PM +0530

*Dears*
* Materials P11,P91 & LTCS.*
* Is there any provision to perform PWHT after Hydrotest without having to
repeat the Hydrotest again ?*
 
*THANKS & BEST REGARDS,*
*KG.PANDITHAN, BE, ...more
sridhar cn <sridharcn305@gmail.com>: Jul 17 07:46PM +0530

*For main pressure welds on materials like P11, P91, and LTCS, **PWHT is
essential when prescribed, and the integrity test (hydro) *
*must **follow all heat treatments unless the code or a ...more
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANeLWoPGe27rKvsjd%2BKVMBrx-eC6VgtkBVo51nigd473d4h5NQ%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...