Sunday, January 12, 2025

Re: [MW:35380] MECHNICAL Testing sample

dear sir,

for casting & forging- standard test bar is enough for conducting mechanical testing 
for plate - we can take mechanical test sepecimen size as per ASME sec IX sample picture 
 

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


On Saturday 28 December, 2024 at 11:14:09 pm IST, Chandrapal Singh <avioraio@gmail.com> wrote:


How to select sample size for mechanical testing for different material (casting , rolled plate forging)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJDZhX8Hw7vp3C89JM_%2BV8vqTziKrHVjhNg_ZPytTZnY-vTzfA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...