Thursday, December 26, 2024

Re: [MW:35361] Application of Non PWHT WPS to PWHT vessel

ASME SEC 9, QW 407.1

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Dec 19, 2024 at 5:53 PM Vasagan Balaji <7vasagan@gmail.com> wrote:
Than you pandithan , noted ! But what's reference for same ?

Regards 

On Thu, 19 Dec 2024 at 1:12 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
new pqr  to be made with vessels simulation temp, hope so
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Dec 19, 2024 at 3:24 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:

When all other essential variables are same , except PWHT , you have to revise WPS  with PWHT and do further needful in consultation with AI 

Thanks
Vishwas 
IWE

Sent from my iPhone

On 19 Dec 2024, at 10:52 AM, Vasagan Balaji <7vasagan@gmail.com> wrote:

Hello all,

I have a case for a U stamp vessel , Vessel designed initially with  no PWHT,  hence non PWHT wps applied throughout the production phase,  later the manufacturer converted vessel requirement to PWHT ! Manufacturer justifies since all other patemerts met the requirement othethan  PWHT , they intent to proceed for PWHT ! What's ASME position shall be here ?


Regards 

Vasagan 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKV0Q%2Bj0HY_TWzxxXbAnt%2Bm-QXHXVE5xgGfBAgKc4QSQDtq5tg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/6F63C283-5709-4107-907A-DA0EDA402D36%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOyaYkYq6QorDUQy7QkQpd6fyMVdYimRanKaYHX__sJKA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKV0Q%2BgDBNm2jEz-ALVsDmW6WifbzfhV%2BH15auL8widRSB5%3DPg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNiF5TieE6mVL1k7D0fZFzDbDZR%3Dz9eVeap%3DK3e%2BAtsDg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...