Monday, December 16, 2024

Re: [MW:35338] Need suggestion

Dear Chirag,

It depends on the material and the minimum temperature mentioned in ASME B31.3 (if applicable).

for CS material  criteria to be defined based on the Table 323.2.2 of applicable 31.3 code.


Thanks
Sharief

On Fri, Dec 13, 2024 at 5:42 PM Chirag Patel <chiragp1985@gmail.com> wrote:
I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/b7446104-f741-424e-8d98-669afa38f068n%40googlegroups.com.


--

Kind Regards,

 

Muhammed Sharief

QC Supervisor

Tamimi Industrial Services

(Branch of Tamimi Global Co. Ltd.)

Tel: +966 13 341 1391 Ext. 3228

Mobile: +966 539141980

E Mail : mpazhadathil@al-tamimi.com

Website: www.tamimi-tis.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAL2iHPsYd_wy_YAJmehM%2BsNdFoNTM5UpcsxAW8-%3DUZgGJHYs9Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...