Monday, December 16, 2024

Re: [MW:35340] Need suggestion

Also specify the Design Code such as ASME B31.3;  -29degC is a general cutoff for carbon steels such as a106Gr.B, A105 etc..

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday 14 December, 2024 at 05:59:09 pm IST, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


It will be decided based on Thickness, Material specification as sometimes there may be Base Material Impact exemptions.


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday 14 December, 2024 at 02:01:39 pm IST, 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> wrote:


No
 you are allowed to use said wps for welding of job having mdmt -20c and warmer
Hegde


On Fri, 13 Dec 2024 at 20:12, Chirag Patel
<chiragp1985@gmail.com> wrote:
I am having WPS impact temperature range with -20 degree. Can i do the welding for -29 degree impact requirement job as per ASME code 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/b7446104-f741-424e-8d98-669afa38f068n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1455130636.2008996.1734164714799%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/586507239.727069.1734168307070%40mail.yahoo.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...