Dear sir
Check your drawing about thickness and MDMT 

Refer UCS 66 and check 

Sent from my iPhone

On 15 Dec 2024, at 1:19 PM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Provided welding consumable guaranteed impact tested as per ASME SecIIC


On Sun, 15 Dec 2024 at 13:13, 'james gerald' via Materials & Welding
<materials-welding@googlegroups.com> wrote:
No impact test required



On Fri, 13 Dec 2024 at 20:11, Chirag Patel
<chiragp1985@gmail.com> wrote:

Dear All,

Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX

Material  to be used used during Fabrication - SA 516 Gr 70

Production Thickness range-8 mm(Minimum)- 20mm(Maximum)
PWHT – Nil
MDMT-= -29 Deg Cel.
Kindly give your valuable suggestions for applicability of PQR impact requirement for above details.
Pl.reply with code clause.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/73179f68-79bc-4185-9aa5-f696add58852n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/211530362.847681.1734248493634%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1855906062.1311416.1734248814585%40mail.yahoo.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...