Re: [MW:35194] Dressing # Grinding ( PQR & wqt )

On weld caping dressup not effect for mechanical testings. Weld caping (above based metal) consider as excessive material. So we can allow start ,stop point dressup.
On this case code is silent.


On Tue, 27 Aug 2024, 6:51 pm Dinesh Baskaran, <dinesh09nov@gmail.com> wrote:
Dear sir 

During PQR /wqt - has welder allow to do small correction ON WELD BEAD , during welding, ( stat AND stop points)  
#Where code mention Regarding this dressing
( ASME SEC9, D1.1, ANY OTHER CODES ) 

Pls kindly share your inputs 

Thank and regards
Dinesh Baskaran
   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVq30%3DhO%3D6XW%2BTGGMhnF8QQf7D3VjX-U33jC1Pc_41v7hg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKnOyb6DVjMNEBA6jgC%2BtwvAdF6QE0ek3fHGjcS%2BnV_cHQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...