You may use ISO 15614 for Procedure qualification and ISO 9606 for welder qualification.

Thanks & Regards,

 

Raviraj Gohil | Manager - Welding | + 83473 02025 | www.lloydsengg.in 




On Thu, Aug 22, 2024 at 3:40 PM Ganesh R nair <ganeshrnair9@gmail.com> wrote:
Dears,

Which ISO standard shall be followed for qualification of WPS and Welders on Alu Zinc material (2mm).

Thanks and regards,
Ganesh R Nair

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJUHeMm2pPD9aVB0qSk3b3Gi%3DrFw4zvPwYG5kdpOGs3CPw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BN2U4MygX44tZHXOxcvDMNPDdMxr0DEUrhAan1cg5p0Jcr-vA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...