Wednesday, August 28, 2024

[MW:35193] Dressing # Grinding ( PQR & wqt )

Dear sir 

During PQR /wqt - has welder allow to do small correction ON WELD BEAD , during welding, ( stat AND stop points)  
#Where code mention Regarding this dressing
( ASME SEC9, D1.1, ANY OTHER CODES ) 

Pls kindly share your inputs 

Thank and regards
Dinesh Baskaran
   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVq30%3DhO%3D6XW%2BTGGMhnF8QQf7D3VjX-U33jC1Pc_41v7hg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...