Thursday, November 30, 2023

Re: [MW:34662] Re: Pitting Corrosion Test ASTM G48 Method A for SS 316L Materials

Just to share. Below snap shot.

Inline image


Thanks & Regards

J.Gerald Jayakumar


On Thursday, 30 November, 2023 at 02:18:30 pm IST, james gerald <gerry_tup@yahoo.com> wrote:


This seems surprising Client specification calling for G48A Terst for 316L. What is the service and what is the level of Chloride ppm in service. What is the PREN requirement.

Please share the Snap shot of Client spec.

Tn Wednesday, 29 November, 2023 at 07:19:44 pm IST, Stephenraj <arokkiyaraj@gmail.com> wrote:



It is raw material Seam less 316L pipe 

On Wed, Nov 29, 2023, 12:05 Ashish Chacko <iamashleo007@gmail.com> wrote:
Can u let us know what was the type of material pipe or plate or whether it was welded?

On Tuesday, 28 November 2023 at 20:18:54 UTC+3 stephen raj wrote:
Dear Sir,
For SS316L material, we performed the Pitting Corrosion Test ASTM G48 Method A in accordance with the client's specifications and acceptance criteria, and we followed ISO 17781 standards in accordance with the client's standard reference.


We failed the test, and the weight reduction ranged from 50 to 500 g. It should be 1g according to the standard.


Can somebody advise or explain why this test failed?

BR

Stephenraj.s

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/900b818a-eb0e-4641-a0a6-563ec5004802n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMugN4ntPtd9LLwmny7cwFo5xwLxuoX83bVpfsDLhmNuN3oTpw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...