E71T stands for flux core wire or tubular electrodes as per AWS. C stands for carbon dioxide as shielding gas and M stands for Argon+CO2 as shielding gas general (70+30)% or (75+25)% respectively.

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Kannayeram Gnanapandithan
Sent: Friday, November 24, 2023 7:46 PM
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:34646] Filler

 

both are except usage of shielding gas. C- For 100%CO2. M- Mixed gas. example Argon plus Co2 etc

 

On Fri, Nov 24, 2023, 9:16 PM Elayaraja Thangarasu <elayaraja1312@gmail.com> wrote:

Dear All.

 

 What is the difference E71T-1C and E71T-1M.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMsS8imTvKcoyfMPr43Wc7uex78s%3De0gOJ_JF8fKHnY_XKa19Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN6qvecbhhm5BSszLydnz2Pm9RDApK-NvTr6Rcz7yRr4g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...