Re: [MW:34641] Interpass Temprature

asme sec 1

On Fri, Nov 24, 2023, 5:28 PM Ashish Chacko <iamashleo007@gmail.com> wrote:

Dear Sirs,

I have inquiries regarding the comprehension of interpass temperature in ASME :

  1. 1)What code reference is used to ascertain the maximum interpass temperature?
  2. 2)What code reference is employed to establish the interpass temperature for dissimilar welds, such as CS to SS welds?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c2f3530-e9f7-4d0f-a51f-40f799445bdbn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM1RBjTWAY8w4r6QwEgq1o4ANmNx5J-pg_p8etifAnM8w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...