Re: [MW:34636] Kind Consideration of API-650 expert is required

API 650 also lists EN ISO materials in section 4.2, below snap shot.

Inline image
S355 JR is not listed but can be impact tested to suit code requirements.

Moreover Anchor chairs falls under structural shapes in which S275 JR is a listed material and you try to get exemption from Designer for the use of higher strength S355JR.


Inline image


On Thursday, 16 November, 2023 at 02:43:15 pm IST, Muiz Azhar <abdulmuizrdx@gmail.com> wrote:


Our exact case is, we want to use S355-JR material for the anchor chair assembly, the assembly shall be prepared using the plate material except anchors. Since S355-JR is not a listed plate material as per clause 4.2. Other Codes such as ASME Section VIII-1 does not enlist the material specifications for non-pressure parts, so using the same analogy I posted the query that it seems to me 4.2 is applicable to the wetted parts and may not be applicable to anchor chair. 

On Thursday, 16 November 2023 at 13:50:50 UTC+5 james gerald wrote:
Yes. Refer 4.4 for structural steels.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 16 November, 2023 at 11:45:47 am IST, Muiz Azhar <abdulm...@gmail.com> wrote:


(1) Do the requirements of clause 4.2 of API-650 apply to pressure parts only?

(2) What are the material requirements of API-650 for non-pressure parts?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/cde559d1-37b6-455a-944a-913a1028a58fn%40googlegroups.com
.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...