Our exact case is, we want to use S355-JR material for the anchor chair assembly, the assembly shall be prepared using the plate material except anchors. Since S355-JR is not a listed plate material as per clause 4.2. Other Codes such as ASME Section VIII-1 does not enlist the material specifications for non-pressure parts, so using the same analogy I posted the query that it seems to me 4.2 is applicable to the wetted parts and may not be applicable to anchor chair. 

On Thursday, 16 November 2023 at 13:50:50 UTC+5 james gerald wrote:
Yes. Refer 4.4 for structural steels.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 16 November, 2023 at 11:45:47 am IST, Muiz Azhar <abdulm...@gmail.com> wrote:


(1) Do the requirements of clause 4.2 of API-650 apply to pressure parts only?

(2) What are the material requirements of API-650 for non-pressure parts?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/834957f8-1d87-496f-8ab9-8067133a545fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cde559d1-37b6-455a-944a-913a1028a58fn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...