Thursday, November 16, 2023

Re: [MW:34634] Kind Consideration of API-650 expert is required

Yes. Refer 4.4 for structural steels.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 16 November, 2023 at 11:45:47 am IST, Muiz Azhar <abdulmuizrdx@gmail.com> wrote:


(1) Do the requirements of clause 4.2 of API-650 apply to pressure parts only?

(2) What are the material requirements of API-650 for non-pressure parts?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/834957f8-1d87-496f-8ab9-8067133a545fn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...